1. Preparing to execution piece
Fiberglass parts are obtained by rolling the hand (contact process) by successive layers of fiberglass impregnated with polyester resin, or combination of chopping machine and applied to fiber (polispray), the molds.
READ MORE ...........................
2. Application gelcoat over mold
Most recommended for execution gelcoat fiberglass parts is gelcoat translucent isophthalic with neopentilglicol, it has a good toughness, very bright, high resistance to marine conditions, and does not absorb water. Usually, it uses white pigment.
Gelcoat is ready for use after adding the percentage of hardener (methyl ethyl ketone peroxide).
Gelcoat is ready for use after adding the percentage of hardener (methyl ethyl ketone peroxide).
READ MORE ...........................
3.Tips
Gelcoatul be mixed before use (10 minutes to 24 hours). A low viscosity will cause excessive mixing, increasing the risk of flow and the porosity formation.
READ MORE ...........................
4. Lamination
The first layer of reinforcement layer is stratimat 300 g / mg powder. Be applied after the gelcoat has hardened layer (between 30 min and an hour, but no more).
Resin applied over gelcoat spray strengthened by your age or with a brush, roller or lamb leather. Should apply a thick and smooth, if it can double in weight over ranfort. The first layer of resin and fiber moisten be pressed to follow the contour model without double layers, cuts or scratches.
READ MORE ...........................
5. Removing mold from the model
If the model surface is resistant to styrene monomer and if wax was carefully should not experience problems in removing the mold from the model. Linking ejectorii the compressed air, mold can be removed from the model.
READ MORE ...........................